References
1. G. Bozzolo, R. D. Noebe, J. Ferrante and C. Amador, "An
introduction to the BFS method and its use to model binary NiAl
alloys", Journal of Computer-Aided Materials Design, Vol.6,
1999, pp. 1-32.
2. N. Saunders and A. P. Miodownik, CALPHAD (Calculation of
Phase Diagrams): A Comprehensive Guide, Pergamon, Oxford ; New
York, 1998.
3. L. Q. Chen and Y. Z. Wang, "The continuum field approach
to modeling microstructural evolution", Jom-Journal of
the Minerals Metals & Materials Society, Vol.48, 1996, pp.
13-18.
4. J. C. Zhao, "A Combinatorial Approach for Structural
Materials", Advanced Engineering Materials, Vol.3, 2001,
pp. 143-147.
5. R. W. Cahn, "Rapid Alloy Assessment", Nature, Vol.410,
2001, pp. 643-644.
6. V. Venugopalan and L. Q. Chen, "3D Simulation of Coarsening
of Gamma-Prime Precipitates in a Ni-Al Alloy", A. Gonis,
P. E. A. Turchi, A. J. Ardell, Eds., Nucleation and Growth Processes
in Materials, Boston, MA, MRS, 2000, pp. 327-332.
7. N. Akaiwa and P. W. Voorhees, "Large scale numerical
simulation of microstructural evolution in elastically stressed
solids", Materials Science and Engineering a-Structural
Materials Properties Microstructure and Processing, Vol.285,
2000, pp. 8-12.
8. R. A. Mackay and M. V. Nathal, "Gamma-' Coarsening in
High-Volume Fraction Nickel-Base Alloys", Acta Metallurgica
Et Materialia, Vol.38, 1990, pp. 993-1005.
9. R. W. Hyland, R. Asta, S. M. Foiles and C. L. Rohrer, "Al(fcc):
Al3Sc(L1(2)) interphase boundary energy calculations",
Acta Materialia, Vol.46, 1998, pp. 3667-3678.
10. J. E. Osburn, M. J. Mehl and B. M. Klein, "1st-Principles
Calculation of the Elastic-Moduli of Ni3al", Physical Review
B, Vol.43, 1991, pp. 1805-1807.
11. A. V. Ruban and H. L. Skriver, "Calculated site substitution
in ternary gamma'-Ni3Al: Temperature and composition effects",
Physical Review B, Vol.55, 1997, pp. 856-874.
12. M. Sluiter and Y. Kawazoe, "A study of the thermodynamics
of segregation and partial order at (111) antiphase boundaries
in Ni3Al", Philosophical Magazine a-Physics of Condensed
Matter Structure Defects and Mechanical Properties, Vol.78,
1998, pp. 1353-1364.
13. A. van de Walle, G. Ceder and U. V. Waghmare, "First-principles
computation of the vibrational entropy of ordered and disordered
Ni3Al", Physical Review Letters, Vol.80, 1998, pp. 4911-4914.
14. C. Wolverton and D. Defontaine, "Site Substitution
of Ternary Additions to Ni3al (Gamma') From Electronic-Structure
Calculations", Physical Review B, Vol.49, 1994, pp. 12351-12354.
15. J. H. Xu, B. I. Min, A. J. Freeman and T. Oguchi, "Phase-Stability
and Magnetism of Ni3al", Physical Review B, Vol.41, 1990,
pp. 5010-5016.
16. C. Wolverton, First-principles theory of coherent precipitation
in size- mismatched, in Intergranular and Interphase Boundaries
in Materials, Iib98 1999, vol. 294-2, pp. 469-472.
17. C. Wolverton, "First-principles prediction of equilibrium
precipitate shapes in Al-Cu alloys", Philosophical Magazine
Letters, Vol.79, 1999, pp. 683-690.
18. C. Wolverton, "First-principles theory of 250 000-atom
coherent alloy microstructure", Modelling and Simulation
in Materials Science and Engineering, Vol.8, 2000, pp. 323-333.
19. C. Woodward, S. Kajihara and L. H. Yang, "Site preferences
and formation energies of substitutional Si, Nb, Mo, Ta,and
W solid solutions in L1(0) Ti-Al", Physical Review B, Vol.57,
1998, pp. 13459-13470.
20. C. Woodward, M. Asta, G. Kresse and J. Hafner, "Density
of constitutional and thermal point defects in L1(2) Al3Sc -
art. no. 094103", Physical Review B, Vol.6309, 2001, pp.
4103-+.
21. L. Kaufman and H. Bernstein, Computer Calculation of Phase
Diagrams with Special Reference to Refractory Metals, Academic
Press, New York, 1970.
22. I. Ansara and B. Sundman, "The Scientific Group Thermodata
Europe", P. S. Glaeser, Ed., Computer Handling and Dissemination
of Data, Elsevier Science Pub. Co, 1987, pp. 154-158.
23. A. T. Dinsdale, "SGTE Data for Pure Elements",
CALPHAD, Vol.15, 1991, pp. 317-425.
24. B. Sundman and J. Agren, "A Regular Solution Model
for Phases with Several Components and Sublattices, Suitable
for Computer Applications", J. Phy. Chem Solids, Vol.42,
1981, pp. 297-301.
25. J. O. Andersson, A. F. Guillermet, M. Hillert, B. Jansson
and B. Sundman, "A Compound-Energy Model of Ordering in
a Phase With Sites of Different Coordination Numbers",
Acta Metall., Vol.34, 1986, pp. 437-445.
26. W. Huang and Y. A. Chang, "A thermodynamic analysis
of the Ni-Al system", Intermetallics, Vol.6, 1998, pp.
487-498.
27. Z. K. Liu and Y. A. Cheng, "Thermodynamic assessment
of the Co-Ta system", Calphad-Comput. Coupling Ph. Diagrams
Thermochem., Vol.23, 1999, pp. 339-356.
28. Z. K. Liu and Y. A. Chang, "Evaluation of the thermodynamic
properties of the Re-Ta and Re- W systems", J. Alloy. Compd.,
Vol.299, 2000, pp. 153-162.
29. G. L. Erickson, "The development and application of
CMSX-10", R. D. Kissinger, et al., Eds., Superalloys 1996,
Champion, Pennsyslvania, USA, Minerals, Metals and Materials
Society/AIME, 1996, pp. 35-44.
30. W. Huang and Y. A. Chang, "A thermodynamic description
of the Ni-Al-Cr-Re system", Mater. Sci. Eng. A, Vol.259,
1999, pp. 110-119.
31. C. Jia, K. Ishida and T. Nishizawa, "Experimental and
thermodynamic analysis on phase equilibria of Ni- rich region
in Ni-Al-Ti system", Rare Metals (English Edition) (China),
Vol.19, 2000, pp. 110-117.
32. J.-O. Andersson, L. Hoglund, B. Jonsson and J. Agren, "Computer
Simulation of Multicomponent Diffusional Transformations in
Steel", G. R. Purdy, Ed., Fundamentals and Applications
of Ternary Diffusion, Pergmon Press, 1990, pp. 153-163.
33. B. Jonsson, "Assessment of the Mobilities of Cr, Fe,
and Ni in Fcc Cr-Fe-Ni Alloys", Z. Metallkd., Vol.86, 1995,
pp. 686-692.
34. B. Jonsson, "Mobilities in Fe-Ni Alloys - Assessment
of the Mobilities of Fe and Ni in Fcc Fe-Ni Alloys", Scand.
J. Metall., Vol.23, 1994, pp. 201-208.
35. A. Engstrom and J. Agren, "Assessment of Diffusional
Mobilities in Face Centered Cubic Ni-Cr-Al Alloys", Z.
Metallkd., Vol.87, 1996, pp. 92-97.
36. M. Fahnle, B. Meyer, J. Mayer, J. S. Oehrens and G. Bester,
"Diffusion in Metals and Intermetallic Compounds: The Impact
of Ab- Initio Calculations", Y. Mishin, G. Vogl, N. Cowern,
R. Catlow, D. Farkas, Eds., Diffusion Mechanisms in Crystalline
Materials, Boston, Materials Research Society, 1998, pp. 23-34.
37. Y. Wang, D. Banerjee, C. C. Su and A. G. Khachaturyan, "Field
kinetic model and computer simulation of precipitation of Ll(2)
ordered intermetallics from FCC solid solution", Acta Materialia,
Vol.46, 1998, pp. 2983-3001.
38. A. G. Khachaturyan, Theory of Structural Transformations
in Solids, John Wiley & Sons, New York, 1983.
39. L. Q. Chen and J. Shen, "Applications of semi-implicit
Fourier-spectral method to phase field equations", Computer
Physics Communications, Vol.108, 1998, pp. 147-158.
40. J. Z. Zhu, L. Q. Chen, J. Shen and V. Tikare, "Coarsening
kinetics from a variable-mobility Cahn-Hilliard equation: Application
of a semi-implicit Fourier spectral method", Physical Review
E, Vol.60, 1999, pp. 3564-3572.
41. S. Y. Hu and L. Q. Chen, "An Efficient Diffuse-Interface
Model for Elastically Anisotropic Systems with Significant Modulus
Inhomogeneity", Acta Materialia, Vol.Accepted, 2001, pp.
.
42. S. Y. Hu and L. Q. Chen, "Solute segregation and coherent
nucleation and growth near a dislocation - A phase-field model
integrating defect and phase microstructures", Acta Materialia,
Vol.49, 2001, pp. 463-472.
43. Y. U. Wang, U. M. Jin, A. M. Cuitino and A. G. Khachaturyan,
"Nanoscale Phase Field Theory of Dislocations: Model and
3D Simulations", Acta Materialia, submitted, 2001, pp.
.
44. B. J. Peiarcey and C. K. Bullough, "An On-Line Materials
Database for Design of Gas Turbine Components", Presented
at the International Gas Turbine & Aeroengine Congress &
Exhibition, Orlando, FLJune 2-5, 1997
45. D. A. Woodford, "Parametric Analysis of Monocrystalline
CMSX-4 Creep and Rupture Data", Metallurgical Transactions
A, Vol.29, 1998, pp. 2645.
46. R. M. Goldhof, Ed., The Evaluation of Elevated Temperature
Creep and Rupture Strength Data: An Historical Perspective,
Characterization of Materials for Service at Elevated Temperatures,
ASME, New York, 1968.
47. S. S. Manson, Ed., Time-Temperature Parameters - A Re-evaluation
and Some New Approaches, Time-Temperature Parameters for Creep
Rupture Analysis, ASM, Metal Park, OH, 1969.
48. S. Tin, T. Pollock and W. Murphy, "Carbon Additions
and Their Influence on Grain Defect Formation in Ni-base Single
Crystals", TMS-AIME Fall Meeting, Cincinnati, OH1999
49. A. R. Price and B. A. Mueller, "Advances in Casting
Large Single Crystal Components for Industrial Gas Turbines",
TMS-AIME Fall Meeeting, Cincinnati, Ohio1999
50. M. Konter, M. Newnham and C. Tonnes, Monocrystalline Nickel-Base
Superalloys with Ti, Ta and Hf Carbides, U.S. Patent 5,759,301.
(U.S., 1998).
51. D. M. Shah and D. N. Duhl, Eds., Effect of Minor Elements
on the Deformation Behavior of Ni-Base Superalloys, Superalloys